Lowest Price for China Arc SmCo Segment Samarium Cobalt Motor Magnets
We emphasize enhancement and introduce new solutions into the market just about every year for Lowest Price for China Arc SmCo Segment Samarium Cobalt Motor Magnets, Our professional technical team will be wholeheartedly at your service. We sincerely welcome you to visit our website and company and send us your inquiry.
We emphasize enhancement and introduce new solutions into the market just about every year forChina Arc SmCo Magnets,Segment Magnets, We warmly welcome you to come to visit us personally. We hope to establish a long-term friendship based on equality and mutual benefit. If you want to get in touch with us, be sure to do not hesitate to call. We are going to be your best choice.
Introduction:
SmCo magnets represent the latest generation of magnetic materials. They are developed over 40 years ago and introduced the era of permanent magnet motors. At that time, these rare earth metals were very expensive. During the 1980s, SmCo material was increasingly replaced by NdFeB magnets. Due to the dramatic price rise in the rare earths neodymium and dysprosium (Nd/Dy), this material has now regained its popularity in applications at higher temperatures (150°C – 200°C). However, there are limits set on the material with regard to the maximum remanence. Two major types of SmCo magnets are available, 1:5 type (SmCo5) and 2:17 type (Sm2Co17). SmCo magnets have super high magnetic properties and temperature properties.
Advantage:
Use of these magnets is conditioned by the temperature in a wide range running from 250ºC to 350ºC and their Curie temperature can be as high as 710 to 880 °C. Therefore, SmCo magnet has the best magnetic stability due to the superior resistance to high temperature. SmCo magnets are characterized by very high corrosion resistance, no coating required for surface protection.
Feature:
A disadvantage of SmCo magnets is the marked brittleness of the material – a factor which must be particularly taken into account during processing. The magnets are galvanized or coated by cathodic electrodeposition for certain applications.
Application:
In areas high operating temperature, high corrosion and oxidation resistance are crucial. Such as Electronic magnetron, Magnetic transmission, Magnetic treatment, Magnistor, etc.
All stated values were determined using standard samples according IEC 60404-5. The following specifications serve as reference values and may differ. The max. operating temperature is
dependent on the magnet dimesion and the specific application. For more information please
contact our application engineers.
Sintered SmCo Magnet Physical Properties | |||||||||
Material | Grade | Remanence | Rev. Temp.- Coeff. Of Br | Coercive Force | Intrinsic Coercive Force | Rev. Temp.-Coeff. Of Hcj | Max. Energy Product | Max. Operating Temperature | Density |
Br (KGs) | Hcb (YOU) | Hcj (YOU) | (BH)max. (MGOe) | g/cm³ | |||||
SmCo5 | XG16 | 8.1-8.5 | -0.050 | 7.8-8.3 | 15-23 | -0.30 | 14-16 | 250℃ | 8.3 |
XG18 | 8.5-9.0 | -0.050 | 8.3-8.8 | 15-23 | -0.30 | 16-18 | 250℃ | 8.3 | |
XG20 | 9.0-9.4 | -0.050 | 8.5-9.1 | 15-23 | -0.30 | 19-21 | 250℃ | 8.3 | |
XG22 | 9.2-9.6 | -0.050 | 8.9-9.4 | 15-23 | -0.30 | 20-22 | 250℃ | 8.3 | |
XG24 | 9.6-10.0 | -0.050 | 9.2-9.7 | 15-23 | -0.30 | 22-24 | 250℃ | 8.3 | |
XG16S | 7.9-8.4 | -0.050 | 7.7-8.3 | ≥23 | -0.28 | 15-17 | 250℃ | 8.3 | |
XG18S | 8.4-8.9 | -0.050 | 8.1-8.7 | ≥23 | -0.28 | 17-19 | 250℃ | 8.3 | |
XG20S | 8.9-9.3 | -0.050 | 8.6-9.2 | ≥23 | -0.28 | 19-21 | 250℃ | 8.3 | |
XG22S | 9.2-9.6 | -0.050 | 8.9-9.5 | ≥23 | -0.28 | 21-23 | 250℃ | 8.3 | |
XG24S | 9.6-10.0 | -0.050 | 9.3-9.9 | ≥23 | -0.28 | 23-25 | 250℃ | 8.3 | |
Sm2Co17 | XG24H | 9.5-10.2 | -0.025 | 8.7-9.6 | ≥25 | -0.20 | 22-24 | 350℃ | 8.3 |
XG26H | 10.2-10.5 | -0.030 | 9.4-10.0 | ≥25 | -0.20 | 24-26 | 350℃ | 8.3 | |
XG28H | 10.3-10.8 | -0.035 | 9.5-10.2 | ≥25 | -0.20 | 26-28 | 350℃ | 8.3 | |
XG30H | 10.8-11.0 | -0.035 | 9.9-10.5 | ≥25 | -0.20 | 28-30 | 350℃ | 8.3 | |
XG32H | 11.0-11.3 | -0.035 | 10.2-10.8 | ≥25 | -0.20 | 29-32 | 350℃ | 8.3 | |
XG22 | 9.3-9.7 | -0.020 | 8.5-9.3 | ≥18 | -0.20 | 20-23 | 300℃ | 8.3 | |
XG24 | 9.5-10.2 | -0.025 | 8.7-9.6 | ≥18 | -0.20 | 22-24 | 300℃ | 8.3 | |
XG26 | 10.2-10.5 | -0.030 | 9.4-10.0 | ≥18 | -0.20 | 24-26 | 300℃ | 8.3 | |
XG28 | 10.3-10.8 | -0.035 | 9.5-10.2 | ≥18 | -0.20 | 26-28 | 300℃ | 8.3 | |
XG30 | 10.8-11.0 | -0.035 | 9.9-10.5 | ≥18 | -0.20 | 28-30 | 300℃ | 8.3 | |
XG32 | 11.0-11.3 | -0.035 | 10.2-10.8 | ≥18 | -0.20 | 29-32 | 300℃ | 8.3 | |
XG26M | 10.2-10.5 | -0.035 | 8.5-9.8 | 12-18 | -0.20 | 24-26 | 300℃ | 8.3 | |
XG28M | 10.3-10.8 | -0.035 | 8.5-10.0 | 12-18 | -0.20 | 26-28 | 300℃ | 8.3 | |
XG30M | 10.8-11.0 | -0.035 | 8.5-10.5 | 12-18 | -0.20 | 28-30 | 300℃ | 8.3 | |
XG32M | 11.0-11.3 | -0.035 | 8.5-10.7 | 12-18 | -0.20 | 29-32 | 300℃ | 8.3 | |
XG24L | 9.5-10.2 | -0.025 | 6.8-9.0 | 8-12 | -0.20 | 22-24 | 250℃ | 8.3 | |
XG26L | 10.2-10.5 | -0.035 | 6.8-9.4 | 8-12 | -0.20 | 24-26 | 250℃ | 8.3 | |
XG28L | 10.3-10.8 | -0.035 | 6.8-9.6 | 8-12 | -0.20 | 26-28 | 250℃ | 8.3 | |
XG30L | 10.8-11.5 | -0.035 | 6.8-10.0 | 8-12 | -0.20 | 28-30 | 250℃ | 8.3 | |
XG32L | 11.0-11.5 | -0.035 | 6.8-10.2 | 8-12 | -0.20 | 29-32 | 250℃ | 8.3 | |
Note: |