Supply ODM China Magnet Bar&Ball Construction Splices Blocks 436PCS
We stick to the principle of “quality to start with, service initially, continual improvement and innovation to meet the customers” for your administration and “zero defect, zero complaints” as the standard objective. To fantastic our service, we offer the products using the very good high quality at the reasonable price for Supply ODM China Magnet Bar&Ball Construction Splices Blocks 436PCS, We’re one from the largest 100% manufacturers in China. Several large trading corporations import goods from us, so we will supply you with the most effective price tag with all the same quality if you are interested in us.
We stick to the principle of “quality to start with, service initially, continual improvement and innovation to meet the customers” for your administration and “zero defect, zero complaints” as the standard objective. To fantastic our service, we offer the products using the very good high quality at the reasonable price forChina Educational Toys and Magnetic Blocks price, Adhering to the principle of “Enterprising and Truth-Seeking, Preciseness and Unity”, with technology as the core, our company continues to innovate, dedicated to providing you with the highest cost-effective products and meticulous after-sales service. We firmly believe that: we are outstanding as we are specialized.
Introduction:
AlNiCo alloys basically consist of aluminum, nickel, cobalt, copper, iron and titanium. In some grades cobalt and/or titanium can be omitted. Also these alloys may contain additions of silicon, columbium, zirconium or other elements which enhance heat treatment response of one of the magnetic characteristics. AlNiCo alloys are formed by casting or powder metallurgical processes.
Feature:
1. AlNiCo magnet has high remanent induction but low coercivity. It works stable at extreme temperature, maintaining its magnetic characteristics between –250ºC and 550ºC. Based on superior magnetic induction, it is largely used in measuring equipment and detection systems.
2. Alnico is a fragile material and can only be altered during the casting process. Orientation of it achieved during heat treatment, producing a magnetic field with the defined magnetization direction.
3. Due to the low coercive force, AlNiCo magnets can be easily affected by reverse magnetic force and impact of iron. That’s why they can be easily demagnetized by external influences. For this reason, AlNiCo magnets should not be stored and packed with the same poles opposing to each other.
4. In open circuit, the ration of length/diameter (L/D) should be at least 4:1. With shorter length,
5. AlNiCo magnets behave well against oxidation. No coating required for surface protection.
Applications:
Use in high sensitivity products such as Instruments, Meters, Mobile Phones, Automobile parts, Electroacoustic devices, Motors, Teaching and Aerospace military, etc.
All stated values were determined using standard samples according IEC 60404-5. The following specifications serve as reference values and may differ.
Cast AlNiCo Magnet Physical Properties | ||||||||
Material | Grade | Remanence | Rev. Temp.-Coeff. Of Br | Coercivity | Rev. Temp.-Coeff. Of Hcj | Max. Energy Product | Max. Operating Temperature | Density |
Br (KGs) | Hcb (YOU) | (BH)max. (MGOe) | g/cm³ | |||||
Isotropic | LN9 | 6.8 | -0.03 | 0.38 | -0.02 | 1.13 | 450℃ | 6.9 |
Isotropic | LN10 | 6.0 | -0.03 | 0.50 | -0.02 | 1.20 | 450℃ | 6.9 |
Isotropic | LNG12 | 7.2 | -0.03 | 0.50 | +0.02 | 1.55 | 450℃ | 7.0 |
Isotropic | LNG13 | 7.0 | -0.03 | 0.60 | +0.02 | 1.60 | 450℃ | 7.0 |
Isotropic | LNGT18 | 5.8 | -0.025 | 1.25 | +0.02 | 2.20 | 550℃ | 7.3 |
Anisotropic | LNG37 | 12.0 | -0.02 | 0.60 | +0.02 | 1.65 | 525℃ | 7.3 |
Anisotropic | LNG40 | 12.5 | -0.02 | 0.60 | +0.02 | 5.00 | 525℃ | 7.3 |
Anisotropic | LNG44 | 12.5 | -0.02 | 0.65 | +0.02 | 5.50 | 525℃ | 7.3 |
Anisotropic | LNG52 | 13.0 | -0.02 | 0.70 | +0.02 | 6.50 | 525℃ | 7.3 |
Anisotropic | LNG60 | 13.5 | -0.02 | 0.74 | +0.02 | 7.50 | 525℃ | 7.3 |
Anisotropic | LNGT28 | 10.8 | -0.02 | 0.72 | +0.03 | 3.50 | 525℃ | 7.3 |
Anisotropic | LNGT36J | 7.0 | -0.025 | 1.75 | +0.02 | 4.50 | 550℃ | 7.3 |
Anisotropic | LNGT32 | 8.0 | -0.025 | 1.25 | +0.02 | 4.00 | 550℃ | 7.3 |
Anisotropic | LNGT40 | 8.0 | -0.025 | 1.38 | +0.02 | 5.00 | 550℃ | 7.3 |
Anisotropic | LNGT60 | 9.0 | -0.025 | 1.38 | +0.02 | 7.50 | 550℃ | 7.3 |
Anisotropic | LNGT72 | 10.5 | -0.025 | 1.40 | +0.02 | 9.00 | 550℃ | 7.3 |
Sintered AlNiCo Magnet Physical Properties | |||||||||
Material | Grade | Remanence | Rev. Temp.-Coeff. Of Br | Coercivity | Coercivity | Rev. Temp.-Coeff. Of Hcj | Max. Energy Product | Max. Operating Temperature | Density |
Br (KGs) | Hcb (KA/m) | Hcj (KA/m) | (BH) max. (KJ/m³) | g/cm³ | |||||
Isotropic | SALNICO4/1 | 8.7-8.9 | -0.02 | 9-11 | 10-12 | -0.03~0.03 | 3.2-4.8 | 750℃ | 6.8 |
Isotropic | SALNICO8/5 | 5.3-6.2 | -0.02 | 45-50 | 47-52 | -0.03~0.03 | 8.5-9.5 | 750℃ | 6.8 |
Isotropic | SALNICO10/5 | 6.3-7.0 | -0.02 | 48-56 | 50-58 | -0.03~0.03 | 9.5-11.0 | 780℃ | 6.8 |
Isotropic | SALNICO12/5 | 7.0-7.5 | -0.02 | 50-56 | 53-58 | -0.03~0.03 | 11.0-13.0 | 800℃ | 7 |
Isotropic | SALNICO14/5 | 7.3-8.0 | -0.02 | 47-50 | 50-53 | -0.03~0.03 | 13.0-15.0 | 790℃ | 7.1 |
Isotropic | SALNICO 14/6 | 6.2-8.1 | -0.02 | 56-64 | 58-66 | -0.03~0.03 | 14.0-16.0 | 790℃ | 7.1 |
Isotropic | SALNICO14/8 | 5.5-6.1 | -0.01 | 75-88 | 80-92 | -0.03~0.03 | 14.0-16.0 | 850℃ | 7.1 |
Isotropic | SALNICO18/10 | 5.7-6.2 | -0.01 | 92-100 | 99-107 | -0.03~0.03 | 16.0-19.0 | 860℃ | 7.2 |
Anisotropic | SALNICO35/5 | 11-12 | -0.02 | 48-52 | 50-54 | -0.03~0.03 | 35.0-39.0 | 850℃ | 7.2 |
Anisotropic | SALNICO 29/6 | 9.7-10.9 | -0.02 | 58-64 | 60-66 | -0.03~0.03 | 29.0-33.0 | 860℃ | 7.2 |
Anisotropic | SALNICO32/10 | 7.7-8.7 | -0.01 | 90-104 | 94-109 | -0.03~0.03 | 33.0-38.0 | 860℃ | 7.2 |
Anisotropic | SALNICO33/11 | 7.0-8.0 | -0.01 | 107-115 | 111-119 | -0.03~0.03 | 33.0-38.0 | 860℃ | 7.2 |
Anisotropic | SALNICO39/12 | 8.3-9.0 | -0.01 | 115-123 | 119-127 | -0.03~0.03 | 39.0-43.0 | 860℃ | 7.25 |
Anisotropic | SALNICO44/12 | 9.0-9.5 | -0.01 | 119-127 | 124-132 | -0.03~0.03 | 44.0-48.0 | 860℃ | 7.25 |
Anisotropic | SALNICO37/15 | 7.0-8.0 | -0.1 | 143-151 | 150-158 | -0.03~0.03 | 37.0-41.0 | 870℃ | 7.2 |
Note:
· We remain the same as above unless specified from customer. Curie temperature and temperature coefficient are for reference only, not as a basis for decision.
· The maximum working temperature of magnet is changeable due to ratio of length and diameter and environment factors.